Følg
Nand Kishor Kumar
Nand Kishor Kumar
Research Scholar, Department of Metallurgical and Materials Engineering, IIT Kharagpur
Verifisert e-postadresse på iitkgp.ac.in
Tittel
Sitert av
Sitert av
År
Effect of twin spacing, dislocation density and crystallite size on the strength of nanostructured α-brass
NK Kumar, B Roy, J Das
Journal of Alloys and Compounds 618, 139-145, 2015
482015
High leaded tin bronze processing during multi-directional forging: Effect on microstructure and mechanical properties
R Gupta, S Srivastava, NK Kumar, SK Panthi
Materials Science and Engineering: A 654, 282-291, 2016
372016
High temperature oxidation response of Al/Ce doped Mo–Si–B composites
J Das, B Roy, NK Kumar, R Mitra
Intermetallics 83, 101-109, 2017
292017
Evolution and interaction of twins, dislocations and stacking faults in rolled α-brass during nanostructuring at sub-zero temperature
B Roy, NK Kumar, PMG Nambissan, J Das
Aip Advances 4 (6), 2014
262014
Effect of Zr addition on microstructure, hardness and oxidation behavior of arc-melted and spark plasma sintered multiphase Mo-Si-B alloys
NK Kumar, J Das, R Mitra
Metallurgical and Materials Transactions A 50, 2041-2060, 2019
212019
Improvement of oxidation resistance of arc-melted Mo76Si14B10 by microstructure control upon minor Fe addition
NK Kumar, B Roy, R Mitra, J Das
Intermetallics 88, 28-30, 2017
162017
Microstructure and High-Temperature Tensile Behavior of Ni-Based Superalloy EP741NP for Aerospace Applications
S Behera, MK Dash, NK Kumar, R Mitra, GA Rao
Journal of Materials Engineering and Performance, 2021
82021
Effect of Fe addition and moist environment on the high temperature oxidation behavior of Mo76-xSi14B10Fex (x = 0, 0.5, 1 at.%) composites
NK Kumar, R Mitra, J Das
Intermetallics 111, 2019
82019
Effect of moist environment on the oxidation behavior of Mo76-xSi14B10Fex (x= 0, 0.5, 1 at.%) ultrafine composites in the range of 700–800° C
NK Kumar, R Mitra, J Das
Corrosion Science 155, 86-96, 2019
52019
Multidirectional forging of high-leaded tin bronze: effect on wear performance
R Gupta, S Srivastava, SK Panthi, NK Kumar
Metallography, Microstructure, and Analysis 6, 577-590, 2017
52017
Effect of Moist Air and Minor Zr Addition on Oxidation Behavior of Arc‑Melted Multiphase Mo–Si–B Alloys in the Temperature Range of 1000 °C–1300 °C
NK Kumar, J Das, R Mitra
Oxidation of Metals, 2020
42020
Multidirectional Forging of High-Leaded Tin Bronze: Evaluation of Corrosion Behavior in Aqueous NaCl Solution
R Gupta, S Srivastava, SK Panthi, NK Kumar
Metallography, Microstructure, and Analysis 7, 11-25, 2018
32018
Systemet kan ikke utføre handlingen. Prøv på nytt senere.
Artikler 1–12